EBSD-assisted fractographic analysis of crack paths in magnesium alloy
Journal Title: Frattura ed Integrità Strutturale - Year 2015, Vol 9, Issue 34
Abstract
Magnesium (Mg) alloys are attractive as structural materials due to their light weight and high specific strength. It is well known that Mg alloy has hexagonal close-packed (HCP) structure and only basal slip or twinning can operate during plastic deformation because critical resolved shear stresses of the other slip systems such as pyramidal or prismatic slips are much higher than the basal slip. Thus sometimes characteristic fracture surfaces are formed during stress corrosion cracking (SCC) or fatigue crack propagation (FCP) in Mg alloys, where many parallel lines are formed. These lines are different from so-called fatigue striations, because they are formed even under sustained load condition of SCC. Consequently, electron back scattered diffraction (EBSD) technique was applied on the fracture surface, and the formation mechanism of parallel lines was investigated. EBSD-assisted fractography had revealed that the characteristic parallel lines were formed due to the operation of basal slips, not twining. It is considered that hydrogen-enhanced localized plasticity (HELP) mechanism had been activated under corrosive environment.
Authors and Affiliations
S. Takaya, Y. Uematsu, T. Kakiuchi
Influence of boundary conditions on the response ofmultilayered plates with cohesive interfaces anddelaminations using a homogenized approach
Stress and displacement fields in multilayered composites with interfacial imperfections, such asimperfect bonding of the layers or delaminations, or where the plies are separated by thin interlayers allowingrelati...
Influence of control parameters on the crack paths in the aluminum alloy 2024 under bending
The paper presents development of crack paths in aluminium alloy 2024. Fatigue tests were carried out for specimens with rectangular cross-section. The specimens were put to bending at controlled energy param...
Combining experimental and numerical analysis to estimate stress fields along the surface crack front
Combining experimental and computational method for determination of the singular and the non-singular stress terms along the front of the 3D surface crack is proposed. Evaluation of the terms is based on comprehen...
L’importanza del “parametro energetico” temperatura per la caratterizzazione dinamica dei materiali
Le esperienze maturate nel campo dell’analisi termica di materiali utilizzati nelle costruzioni meccaniche [1,2,3] hanno permesso di evidenziare come il rilievo della temperatura (terzo parametro) in prove statiche e din...
Plastic flow equations for the local strain approach in the multiaxial case
This paper presents a system of plastic flow equations which uses and generalizes to the multiaxial case a number of concepts commonly employed in the so-called Local Strain Approach to low cycle fatigue. Eve...