Phase transformations and microstructure of IN-713C nickel superalloy
Journal Title: Archiwum Odlewnictwa - Year 2009, Vol 9, Issue 2
Abstract
The study presents the results of investigations of phase transformations taking place during melting and solidification and of microstructural examinations carried out on the family of IN 713C nickel superalloys. Examinations were carried out by the method of thermal analysis (ATD) and differential scanning calorimetry (DSC). It has been concluded that the method of thermal analysis (ATD) enables more precise assessment of the precipitation of the primary phases of a low value of the solidification enthalpy. The advantage of DSC is the possibility of determination of the value of the heat (enthalpy) of phase transformations during alloy melting and solidification. The measured parameters of Tlik and Tsol are comparable for both methods. Microstructural examinations have confirmed the phenomena accompanying phase transformations, i.e. the precipitation of primary carbides, the solidification of delta phase matrix and carbide eutectic, and the formation of delta’ phase in solid state.
Authors and Affiliations
F. Binczyk, J. Śleziona
Bainitic-martensitic nodular cast iron with carbides
In this paper the possibility obtaining of upper bainite, lower bainite and martensite or their mixture in nodular cast iron with carbides has been presented. Conditions have been given, when in nodular cast iron with ca...
The modification process of AlSi21CuNi silumin and its effect on change of mechanical properties of the alloy
Due to difficulties present during machining operations and with segregation of crystals of primary silicon, hypereutectic silumins can be used after modification only. It is why elaboration of effective modification met...
Effect of ring notch radius on the decohesion mode in AlSi alloys
The article discusses the effect of the, determined by tensile test, non-linear characteristics of AlSi alloys on the value of the shape factor k for the three different sizes of the radius of the ring notch made on roun...
Compression effect and the structure of liquid eutectic
ExperimentallyT Tinvestigated theT TtemperatureT Tdependence ofT Tthe densityT and Tthermoelectric power ofT Tthe eutecticT TmeltT. TBased on theT TresultsT TandT Tstructural modeling,T Tto explain the effectT Tof compre...
The thermal analysis and derivative bronzes cast to plaster moulds
It plaster moulds gets casted the alloys of following metals: Al, Cu, Ag, Au in precise and artistic founding. The investigation of the crys-tallization of bronzes in hot plaster moulds the method of the thermal analysis...